Laboratory Techniques and Tube Alloy Ranking to Improve Internal Corrosion Resistance of Automotive Radiators 980056

Internal corrosion resistance of radiators and heaters is becoming more important as automotive manufacturers seek durability past 10 years, and as the usage of aluminum heat exchangers spreads to markets with poorly maintained engine coolant fluid from a corrosion inhibition standpoint. Simulated Service Corrosion Tests (SSCT) are used to evaluate the resistance of three aluminum alloys to tube failure in various corrosive water and depleted coolant conditions. The paper documents results from such tests that lead to two major conclusions: (1.) A weakly inhibited Oyama water solution with a silicated North American engine coolant is highly effective in ranking internal liner alloys for their pitting corrosion resistance, and (2.) AA7072 lined tubes exhibit superior pitting corrosion resistance compared to 1XXX lined tubes. Electrochemical test data obtained in a simulated pit electrolyte and the bulk test solution are utilized to develop an understanding of the SSCT results.

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 16% off list price.
Login to see discount.
Special Offer: Download multiple Technical Papers each year? TechSelect is a cost-effective subscription option to select and download 12-100 full-text Technical Papers per year. Find more information here.
We also recommend:
TECHNICAL PAPER

Brazing Aluminum Automotive Heat Exchanger Assemblies Using a Non-Corrosive Flux Process

830021

View Details

TECHNICAL PAPER

A New Evaluation Method for the Measurement of Internal Corrosion Resistance in Braze Clad Alloys

2002-01-0388

View Details

TECHNICAL PAPER

Method for Predicting and Optimizing the Strength of Extruded Multi-Void Aluminum Heat Exchanger Tube

2001-01-1737

View Details

X