Browse Standards AMS5589F
Historical REVISED 2013-11-07

Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) 0.90Ti - 0.50Al - 18Fe Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated AMS5589F

This specification covers a corrosion and heat-resistant nickel alloy in the form of seamless tubing.
AMS5589G
2019-12-13
Latest
Revised
AMS5589F
2013-11-07
Historical
Revised
AMS5589B
2011-08-12
Historical
Reaffirmed
AMS5589E
2007-07-05
Historical
Revised
AMS5589D
2000-09-01
Historical
Revised
AMS5589C
1994-08-01
Historical
Revised
AMS5589A
1981-04-01
Historical
Revised
AMS5589
1966-09-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 9% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel Alloy, Corrosion and Heat Resistant, Seamless Tubing 72Ni - 15.5Cr - 0.95Cb (Nb) - 2.5Ti - 0.70Al - 7.0Fe Solution Heat Treated, Precipitation Hardenable to 155 ksi (1069 MPa) Tensile Strength

AMS5582G

View Details

STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated

AMS5590G

View Details

STANDARD

Steel, Corrosion- and Heat-Resistant, Seamless or Welded Hydraulic Tubing 18.5Cr - 10.5Ni - 0.40Ti (SAE 30321) Solution Heat Treated

AMS5557K

View Details

Get Involved

Want to participate in updating this standard?

X