Steel, Corrosion and Heat Resistant, Bars, Wire, and Forgings 12.5Cr - Low Carbon (SAE 51416, 51416Se) Free-Machining AMS5610M

This specification covers two types of free-machining, corrosion and heat resistant steel in the form of bars, wire, forgings, and forging stock.
AMS5610R
2023-06-12
Latest
Revised
AMS5610P
2018-07-30
Historical
Revised
AMS5610N
2012-02-09
Historical
Reaffirmed
AMS5610M
2000-10-01
Historical
Revised
AMS5610L
1993-10-01
Historical
Reaffirmed
AMS5610K
1982-07-01
Historical
Revised
AMS5610J
1976-01-01
Historical
Revised
AMS5610H
1973-12-01
Historical
Revised
AMS5610G
1967-04-01
Historical
Revised
AMS5610F
1965-09-01
Historical
Revised
AMS5610E
1952-06-01
Historical
Revised
AMS5610D
1950-06-01
Historical
Revised
AMS5610C
1945-07-01
Historical
Revised
AMS5610B
1944-03-01
Historical
Revised
AMS5610A
1942-06-01
Historical
Revised
AMS5610
1939-12-04
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion Resistant, Sheet and Strip 18Cr - 8Ni (301) Cold Rolled, 125 ksi (862 MPa) Tensile Strength

AMS5517M

View Details

STANDARD

Steel, Corrosion-Resistant, Bars and Forgings 17Cr (0.60 - 0.75C) (440A)

AMS5631F

View Details

STANDARD

Steel, Corrosion-Resistant, Bars and Forgings 0.14S - 18Cr - 9.5Ni - 0.50Mo - 0.80Al (303MA) Free-Machining; Swaging or Upsetting Solution Heat Treated

AMS5638G

View Details

Get Involved

Want to participate in updating this standard?

X