Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Equalized, Precipitation Hardenable AMS5667P

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading.
AMS5667P
2020-08-04
Latest
Revised
AMS5667N
2015-01-07
Historical
Revised
AMS5667M
2008-08-28
Historical
Revised
AMS5667L
2003-06-03
Historical
Revised
AMS5667K
1996-05-01
Historical
Revised
AMS5667J
1990-04-01
Historical
Revised
AMS5667H
1979-07-01
Historical
Revised
AMS5667G
1972-05-01
Historical
Revised
AMS5667F
1960-01-01
Historical
Revised
AMS5667E
1958-08-01
Historical
Revised
AMS5667D
1953-12-01
Historical
Revised
AMS5667C
1951-06-01
Historical
Revised
AMS5667B
1950-06-01
Historical
Revised
AMS5667A
1949-03-01
Historical
Revised
AMS5667
1947-12-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 9% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 74Ni - 15.5Cr - 8.0Fe

AMS5665P

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 47.5Ni - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe Solution Heat Treated

AMS5754N

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated

AMS5709J

View Details

Get Involved

Want to participate in updating this standard?

X