Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened Capable of 160 ksi (1103 MPa) Tensile Strength AMS5853D

This specification covers a corrosion and heat-resistant steel in the form of work-strengthened bars and wire, 1-1/4 inches (31.8 mm) and under in nominal diameter or least distance between parallel sides (see 8.6).
AMS5853E
2024-04-01
Latest
Revised
AMS5853D
2019-02-04
Historical
Revised
AMS5853C
2012-04-13
Historical
Reaffirmed
AMS5853B
2000-10-01
Historical
Revised
AMS5853A
1993-01-01
Historical
Revised
AMS5853
1991-10-01
Historical
Reaffirmed

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.

Get Involved

Want to participate in updating this standard?

X